      But don’t do this. Really. The fdm layers are unhygienic, and there’s a not-insignificant risk of things snapping off and leading to awkward emergency room visits.

      A better solution is printing a 2 part mold and casting silicone.

      • fruitycoder@sh.itjust.works
        link
        fedilink
        English
        arrow-up
        4
        ·
        7 months ago

        I was really impressed by the lulzbot manual mentioning this! Its also important to consider that most 3d prints can be sensitive to water unless sealed too.

        • FuglyDuck@lemmy.world
          link
          fedilink
          English
          arrow-up
          5
          ·
          7 months ago

          I’m just gonna assume some one printed a butplug, had it snap off leading to said emergency room visit and they tried to sue lulzbot.

          • fruitycoder@sh.itjust.works
            link
            fedilink
            English
            arrow-up
            3
            ·
            7 months ago

            Idk lulzbit are also just super consumer freindly out fit (I think are still one the only 3d printer that are FSF Respect Your Freedoms certified).

      • umbrella@lemmy.ml
        link
        fedilink
        English
        arrow-up
        6
        arrow-down
        2
        ·
        edit-2
        7 months ago

        glad to hear from the 3d printed sex toy experts in the house

        wont the layers transfer to the silicone?

        • FuglyDuck@lemmy.world
          link
          fedilink
          English
          arrow-up
          11
          arrow-down
          1
          ·
          7 months ago

          You can process the inside to be smooth (sanding, priming. If you have a solvent - acetone for abs, as an example. And mold release.)

          Even just using a filler/primer should be enough